Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 6.40 mm |
259 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® 193 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 6.40 mm |
259 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® 194 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 945 PC Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | ASTM D648 |
Ravago Manufacturing Americas Hylex® P1032L Polycarbonate, Unreinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HFD4211 PC Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HPS4 PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HPS4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 6.40 mm |
259 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® LSHF PC (Europe-Africa-Middle East) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® R9453 PC (Asia Pacific) Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANTEC PC S90R Polycarbonate Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 6.40 mm |
259 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HF1140 PC (Asia Pacific) Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors. Effective January 15th, 2007 th.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® SFX173RU PC (Asia Pacific) SFX173RU is a transparent SecurFX grade with high flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | |
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 4.00 mm |
259 °F @Thickness 0.157 in |
Unannealed; ASTM D648 |
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp DP003XXP PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DP003XXP is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 3.20 mm |
259 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PC R GY143 Availability: North AmericaForms: PelletsFeatures: Low Smoke EmissionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | Annealed; ISO 75-2/A |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | Annealed; ISO 75-2/A |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 6.40 mm |
259 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 259 °F | ISO 75-1/-2 |
Covestro Makrolon® 1243 Polycarbonate ISO 7391-PC,ELS,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minExtrusionHigh viscosityBranchedUV stabilizedEasy releaseAvailable in color code 550111onlyMulti wall sheet/profilesPreprocessi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C @Thickness 6.40 mm |
259 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® FL1000 PC 5% GR. Various weight reductions at .250""(6.35mm) wall. Excellent flex strength/rigidity, high heat/creep resistance. V-0/5VA rated. |