Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical MA210 ABS, Low Gloss Feature: Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75A |
Lucite International Diakon® ST50G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy Black, Custom Colors. Excellent flame retardancy, easy processability, good impact strength, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS (Asia Pacific) LNP* Thermocomp* CX05470 is a compound based on Polystyrene resin containing Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75 |
Styrolution Novodur® 530 ABS Novodur 530 is an extrusion grade optimized for sheet applications. It has high impact properties, high modulus and good thermoforming.Information provided by Styrolution |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific) LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific) LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.9 °C | 196 °F | ASTM D648 |
Eastman Tritan GX100 Copolyester Eastman Tritan copolyester GX100's strength, clarity and temperature resistance make it ideal for demanding applications. Extruded Sheet is manufactured with Eastman's Tritan copolyester GX100 resi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.35 mm |
196 °F @Thickness 0.250 in |
ASTM D-648 |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers with very low .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.1 °C | 196 °F | 0.25 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3003 MC Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.1 °C | 196 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ASA S950 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ineos Nova 6100 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | |
Arkema Group Oroglas® V 045 I Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 I is an extrusion that exhibits the following properties : 50% tougher than standard acrylics excellent optical properties ( comparable to that of standard acrylics) superior surface .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ineos Nova 6110 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |