Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 20% Glass Fiber Reinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass.
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ASTM D792
1.53 g/cc
0.0553 lb/in³
ISO 1183
Moisture Absorption 0.200 %
0.200 %
50% RH, 24 hrs; ASTM D570
0.340 %
0.340 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.027 - 0.030 cm/cm

@Time 86400 sec
0.027 - 0.030 in/in

@Time 24.0 hour
ASTM D955
0.027 - 0.030 cm/cm

@Time 86400 sec
0.027 - 0.030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.018 - 0.020 cm/cm

@Time 86400 sec
0.018 - 0.020 in/in

@Time 24.0 hour
ASTM D955
0.018 - 0.020 cm/cm

@Time 86400 sec
0.018 - 0.020 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.0 MPa
6090 psi
ASTM D638
44.0 MPa
6380 psi
ISO 527
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D638
44.0 MPa
6380 psi
ISO 527
Elongation at Break 9.7 %
9.7 %
ISO 527
22.9 %
22.9 %
ASTM D638
Elongation at Yield 7.1 %
7.1 %
ISO 527
8.1 %
8.1 %
ASTM D638
Tensile Modulus 3.43 GPa
497 ksi
1 mm/min; ISO 527
3.96 GPa
574 ksi
50 mm/min; ASTM D638
Flexural Strength 70.0 MPa
10200 psi
ISO 178
75.0 MPa
10900 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ISO 178
3.51 GPa
509 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.39 J/cm
10.1 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 37.0 kJ/m²
17.6 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 2.00 J
1.48 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 4.00 J
2.95 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
75.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 79.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
80.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
44.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
91.0 °C

@Thickness 3.20 mm
196 °F

@Thickness 0.126 in
unannealed; ASTM D648