Eastman Tritan GX100 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Tritan
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tritan GX100 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Eastman Tritan copolyester GX100's strength, clarity and temperature resistance make it ideal for demanding applications. Extruded Sheet is manufactured with Eastman's Tritan copolyester GX100 resin in a thickness range from 0.080" to 0.250". It is readily available in clear with colors available upon request.Application/UsesBuilding and constructionDisplaysDurablesElectronicsSignsTransportation and outdoor vehiclesKey AttributesDoes not contain Bisphenol-A (BPA)Does not contain plasticizersEase of fabricationHigh impactTemperature resistanceThermoformingTransparentInformation was provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Water Absorption 0.18 %

@Time 86400 sec
0.18 %

@Time 24.0 hour
Immersion; ASTM D570
Thickness 2970 microns
117 mil
Thickness of film tested; ASTM D374
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength at Break 46.0 MPa
6670 psi
ASTM D638
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 133 %
133 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.483 GPa
215.1 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm

@Temperature -30.0 °C
2.49 ft-lb/in

@Temperature -22.0 °F
ASTM D256
10.06 J/cm

@Temperature 0.000 °C
18.85 ft-lb/in

@Temperature 32.0 °F
ASTM D256
10.11 J/cm

@Temperature 23.0 °C
18.94 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched 12.14 J/cm

@Temperature -30.0 °C
22.74 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
NB

@Temperature 0.000 °C
NB

@Temperature 32.0 °F
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.2 °C
211 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.9 °C
196 °F
ASTM D648
Vicat Softening Point 110 °C
230 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified