Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer Shuman
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Black, Custom Colors. Excellent flame retardancy, easy processability, good impact strength, good chemical resistance, injection molding and extrusion grades.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min
1.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM D638
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
1/8" Thick Specimen; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Flammability, UL94 V-0

@Thickness 1.57 mm
V-0

@Thickness 0.0618 in
5VA

@Thickness 3.18 mm
5VA

@Thickness 0.125 in
Processing Properties Metric English Comments
Processing Temperature 193 - 221 °C
379 - 430 °F
Extrusion
221 - 260 °C
430 - 500 °F
Injection