Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | STN EN ISO 75/A |
Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ASTM D648 |
Nylene® 600 Nylon 6 Dry as molded. Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacke.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANFILL Injection CPC15051 PP/PE, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 75-1/-2 |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | DIN 53461 |
Qualchem Danamid FEWL2-25 Polyamide 6, 25% Mineral Filled Filled with minerals. Flame retardant, with halogens (V-2)Information provided by Qualchem Zrt. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH K20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 - 252 °C | 167 - 486 °F | Average value: 228 °C Grade Count:110 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ASTM D648 |
I. Stern N1841 General Purpose Crystal Polystyrene Features:Excellent Process PropertiesEasy FlowApplicationsDisplaysToys, CosmeticsAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C @Thickness 6.40 mm |
167 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa FRHIPS-702 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | |
LATI Latan 3E71 POM Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | 80x10x4mm; ISO 75-2/Af |
SYNTHOS Krasten® 154 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ASTM Test |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 75 |
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 75-93 |
Wellman Wellamid® NY1615-BK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 75-1, 2 |
Polyplastics Duracon® TD-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ASTM D648 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 75-1,-2 |
Covestro Makroblend® UT5207 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | dry; ISO 75-1/-2 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 PA-66-HWV0CP UL-Licensed Nylon 66, Flame Protection, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
Eurostar Starflam PX06020 PA6, Flame Retardant, Injection Molded Starflam PX06020 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 75 |
BASF Ultramid® A34 01 PA66 (Dry) Ultramid A34 01 is an intermediate visosity, PA66 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ASTM D648 |
Solvay TECHNYL® 2210HS PA66, DRY Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | ISO 75-2/AF |
Addiplast Addinyl B2 G30 Nylon 6, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | |
Radici Radiflam® A AE (dry) Nylon 66 Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |