Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Nylene® NX4301 Nylon 6, Extrusion Grade Dry as molded. Extrusion grade. Nylene NX4301 is a high viscosity, UV stabilized extrusion grade nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance is attri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Proto3000 Accura® Amethyst™ Material for use with Viper™ SLA® systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. FEATURES:Outstanding accuracyExceptional detailHigh thermal resistanceDeep purple colorLow as.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC T12020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP COLORCOMP I1000 PA6.12 LNP* COLORCOMP* I1000 is an unfilled Nylon 6/12 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C @Thickness 6.40 mm |
144 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75/Af |
Solvay TECHNYL® B 230 PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C @Thickness 3.20 mm |
144 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 (Asia Pacific) LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D-648-92 |
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, perm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-1, 2 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75 |
Eastman Drystar 0325 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Drystar 0603 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman PROVISTA Copolymer PETG Copolyester Color, b* CIELAB, Illuminant D6500, 10° Observer is 0.61 per ASTM D 2244.Product Description: PROVISTA Copolymer is a resin specifically developed for extrusion into profiles where aesthetics like.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Provista MP001 Copolymer Provista Copolymer MP001 is a resin specifically developed for extrusion into profiles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Provista UVI Copolymer Provista UVI is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: KK38 is an improved extrusion grade SBC designed specifically for superior performance in blends with general purpose polystyrene. It is easily process.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ISO 75-2/A |
ExxonMobil Exxtral™ CMN 303 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for high heat ageing resistance for automotive interior trim applications such as instrument panels.Availability: Africa & Mi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2/AF |
Addiplast Addilene H 140 Polypropylene Homopolymer Unreinforced, low flow for injection and extrusion, very translucentInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® SC315 NC010 Nylon 612
(Unverified Data**) Zytel® SC315 NC010 is an unreinforced, lubricated 612 polyamide suitable for injection molding. It has been developed for applications such as parts for the healthcare industry.Information provided.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |