Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
Quadrant EPP Duratron® PAI T4203 PAI, unfilled, extruded (ISO Data) Duratron T4203 PAI offers the best toughness and impact strength of all Duratron PAI grades. This extruded Duratron PAI grade is very popular for precision parts in high-tech equipment. In addition,.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
Quadrant EPP Duratron® PAI T4503 PAI, unfilled, compression moulded (ISO Data) Compression moulded Duratron T4503 PAI is similar in composition to Duratron T4203 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | Annealed; ISO 75-2/A |
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | |
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | |
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 280 °C | >= 536 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP LF006EL PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF006EL is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. FDA Compliant Raw Materials. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C @Thickness 6.40 mm |
536 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® XF-4150 PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 280 °C | >= 536 °F | ASTM D648A |
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 280 °C | >= 536 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America E 3812M-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy E 3812M-1 is a mineral and short fiberglass filled epoxy molding compound for low pressure encapsulation molding, featuring excellent dimensional stability, good thermal shock resistance, and good e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 280 °C | >= 536 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America EM 7302XLD Long Glass Fiber Reinforced Epoxy EM 7302XLD is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirable.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | As Molded; ASTM D648A |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C @Thickness 3.20 mm |
536 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON 9X08403C Liquid Crystal Polymer (LCP) LNP* STAT-KON* 9X08403C is a compound based on Liquid Crystal Polymer (LCP) resin containing Carbon Fiber. Added features of this material are: Clean Compounding System, High Temperature, Flame Re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP LX97024 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LX97024 is a compound based on Polyetheretherketone containing Glass Fiber, PTFE. Added features include: Internally Lubricated, Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 280 °C | >= 536 °F | post baked; ASTM D648 |
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Verton OX07411 PPS (Asia Pacific) LNP* Verton* OX07411 is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30 Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50 Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75 |
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | dry; ISO 75-1/-2 |
DSM Stanyl® TW241F5 PA46-GF25 Heat Stabilized, 25% Glass Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® HT1V-4 HY black 9205 PA6T/6I-GF40 Product description: Grivory HT1V-4 HY black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-4 HY bl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 280 °C | 536 °F | As Molded; ASTM D648A |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |