Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 2185 R30 Polyamide + PP Glass fiber reinforcement, 30% Filler by Weight Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Method.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | |
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre FeaturesPET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
Plenco 50130 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 LNP LUBRILOY* RF206 is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material includes: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRILOY RF206AXH PA 66 LNP LUBRILOY* RF206AXH is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material include: Wear Resistant, Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 GF13 FR BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PET GF20 UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RF005 PA 66 LNP* THERMOCOMP* RF005 is a compound based on Nylon 66 resin containing 25% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp RF005 PA 66 (Asia Pacific) LNP* Thermocomp* RF005 is a compound based on Nylon 66 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PET GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ISO 75-1, 2 |
Polyplastics FR-PET® BN9015 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ISO 75 |
Polyram RamSter PE321G6 PET, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant V-0 PET for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
Plenco 6500 Phenolic, Briquette, Transfer Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
Ashley Polymers Ashlene® E128 PET Polyester, 45% Glass Reinforced PET Polyester, economy grade with 45% glass reinforcement.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ISO 75 |
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry) Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
Adell AJ-14 Nylon 66, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
Adell AJ-34 Nylon 66, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 224 °C | 435 °F | ASTM D648 |
Ashley Polymers Ashlene® PE128 PET Polyester, 45% Glass Reinforced PET Polyester, with 45% glass reinforcement.Data provided by the manufacturer |