Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 3.20 mm |
349 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES LNP COLORCOMP* JX91550 is an unfilled Polyethersulfone. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 3.20 mm |
349 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP COLORCOMP JX91550 PES (Asia Pacific) LNP COLORCOMP* JX91550 is a compound based on Polyethersulfone resin containing Unfilled Custom Color. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Plenco 4759 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Global 508 30% Glass Filled PBT Gray Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Lubricomp WFL32 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFL32 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 6.40 mm |
349 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 508 PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 6.40 mm |
349 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 508R PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-FR. Reduced warpage characteristics. Applications same as VALOX 420R. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 3.20 mm |
349 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 3.20 mm |
349 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Asia Pacific) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 3.20 mm |
349 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 3.20 mm |
349 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP PF001S PA 6 (Asia Pacific) LNP* Thermocomp* PF001S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 LNP* THERMOCOMP* SF00A is a compound based on Nylon 12 resin containing 50% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 6.40 mm |
349 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C @Thickness 3.20 mm |
349 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP PF001S PA 6 LNP* THERMOCOMP* PF001S is a compound based on Nylon 6 resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific) Glass filled Nylon 12 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Plenco 2000 Phenolic, Granular, Compression Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Plenco 2311 Phenolic, Granular, Compression Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Plenco 3557 Phenolic, Granular, Compression Molded PLENCO 03557 is a woodflour and mineral filled phenolic molding compound offering excellent dielectric strength values at elevated temperatures while maintaining mechanical strength properties. UL r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | ASTM D648 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 176 °C | 349 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermotuf PF003IX1 PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |