Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 1404 NAT Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | ASTM D648 |
Proto3000 Duraform® GF Selective Laser Sintering (SLS®) Prototyping Polymer Description: Glass-filled polyamide (nylon) material for real-world physical testing and functional useFeatures:Excellent mechanical stiffnessElevated temperature resistanceDimensionally stableEasy-.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | ISO 75 |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 3.20 mm |
273 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON PE002Z PA 6 LNP* STAT-KON* PE002Z is a compound based on Nylon 6 resin containing 10% Carbon Fiber. Added features of this grade include: Extrusion Grade. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP DF0029P PC LNP THERMOCOMP* DF0029P is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Exceptional Processing. Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | ASTM D648 |
Samyang Trirex® 3022A Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | ASTM D648 |
Samyang Trirex® 3022L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | ASTM D648 |
Samyang Trirex® 3022PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022PJ is a general use grade.Information provided by Samyang. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Unannealed; ASTM Data |
Styron CALIBRE™ SF 7070 Polycarbonate, 7% Glass Reinforced Structural Foam Grade CALIBRE® SF7070. is a 7% glass reinforced structural foam ignition resistant polycarbonate resin specially developed for injection molding processing. The CALIBRE 7070 resin provides a high flexu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | |
Aclo Accutech Polycarbonate POL051G10L Glass Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C @Thickness 6.40 mm |
273 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PX2922 PPE (Asia Pacific) GF20% FR-V0 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 134 °C | 273 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® S5220 20% GF PC/ABS alloy Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld .. |