Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | ASTM D648 |
Niche Polymer PPHM6BK Homopolymer PP Information provided by Niche Polymer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | ASTM D648 |
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® ML7647 PC (Europe-Africa-Middle East) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 247 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL NH5120C PPE+PS Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Asia Pacific) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C @Thickness 3.20 mm |
246 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | ISO 75-1, 2 |
Polyplastics TOPAS® 6013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Due to its high transparency, low levels of eluates, superior chemical resistance, and high heat deflection temperature, this grade is suitable for products such as pharmaceutical packaging and diag.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Absolute Drying; ASTM-D648 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | unannealed; ISO 75 |
Chi Mei Wonderloy® PC-385 PC/ABS Alloy Ultra-high Heat, Ultra-high Impact |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | |
BASF Luranyl® KR 2402 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness for parts calling for good heat deformation resistance (e.g. warm-air vents, coil formers, sheet and wheel covers).Data was co.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® EXL1033C PC Copolymer Lexan*EXL1033C polycarbonate (PC) siloxane copolymer resin is a low flow, UV stabilized grade designed for (co)-extrusion. This resin offers low temperature (-30C) ductility and excellent extrusion .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |