Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable E 1400 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W84598L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.Inf.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
Reltek BONDiT™ HM-505 Coating, Sealant, Adhesive System Information provided by Reltek LLC |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
Teknor Apex APEX® 3800-90 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor .. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
Teknor Apex APEX® 80855 Polyvinyl Chloride, Flexible Notes: 90°C Insulation; RoHS CompliantFeatures: Sunlight Resistant (720 hours) Uses: Cable Jacketing; Insulation; Outdoor ApplicationsAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: T.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
Teknor Apex MF 167 NT Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearAgency Ratings- USP Class VIInformation provided.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | |
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing .. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 4770P General Purpose Compound FormulationNordel® IP 4770P |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | Temperature Retraction, TR-10 |
Dow Nordel® IP 4770R General Purpose Compound FormulationNordel® IP 4770R |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GK 89/2 Flexible PVC, Flame Retardant Sheathing Lead Free Special cables |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | |
AlphaGary PVC FM1R Polyvinyl Chloride Thermoplastic Resistant to UV, moisture and mildew for high speed extrusion of coated yarn for outdoors furniture, wire fence coating and automotive harness cable coating |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | Impact Brittleness; ASTM D746 |
Bayshore Vinyl Compounds BVC 6200-85 Vinyl Compound BVC 6200-85 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 17870 Wire & Cable Flexible PVC TW, THW insulation compound. Oil II rated. 720 hour sunlight resistant in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 19910 Wire & Cable Flexible PVC THHN-THWN, best suited for larger sizes (16 AWG and larger).Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 19911 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 19912 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound recommended for various style # applications including 1007 and 1015. The compound is formulated for microbial and fungal resistance.Informatio.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 8850 Moldings & Extrusions Flexible PVC General purpose extrusion.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 19840 Wire & Cable Flexible PVC 105°C rated insulation suitable for 1/64 wall. Recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
Teknor Apex APEX® 3201-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
Teknor Apex APEX® 65009 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3905 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 80/A Flexible PVC, Lead Free Pipes and profiles |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 19935 Wire & Cable Flexible PVC THHN-THWN, larger sizes. Microbe resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 22871 Coax & Telecom Flexible PVC Non-lead, category 5 flexible CMR jacket over HDPE inners.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | Plasticizer conc. in vinyl film 40 phr; ASTM D746 |
BASF Palatinol® N Diisononyl Phthalate Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | |
Sylvin Technologies 5120 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
DuPont Performance Polymers Kalrez® 3065 Fluoroelastomer DuPont™ Kalrez® 3065 is a highly-filled product containing carbon black and fiber reinforcement, designed to function without extrusion under extreme pressure. It has good all round chemical resis.. |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1802L-xx17FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -23.0 °C | -9.40 °F | ASTM D-746 |
Axiall 4900 Flexible PVC Non-lead stabilized, fungus resistant, 105C rated automotive insulation designed to meet the performance criteria of SAE J1128.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |