Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Nordel® IP 4770P General Purpose Compound

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® IP 4770P General Purpose Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FormulationNordel® IP 4770P
Physical Properties Metric English Comments
Density 1.083 g/cc
0.03913 lb/in³
Mooney Viscosity 62

@Temperature 100 °C
62

@Temperature 212 °F
ML 1 + 4
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
Vulcanizate, Press cured, TC95 +3min at 160°C
Tensile Strength, Ultimate 18.8 MPa
2730 psi
Vulcanizate, Press cured, TC95 +3min at 160°C
Elongation at Break 480 %
480 %
Vulcanizate, Press cured, TC95 +3min at 160°C
100% Modulus 0.00390 GPa
0.566 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
200% Modulus 0.00780 GPa
1.13 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
300% Modulus 0.0110 GPa
1.60 ksi
Vulcanizate, Press cured, TC95 +3min at 160°C
Tear Strength 39.3 kN/m
224 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Compression Set 61 %

@Temperature 125 °C
61 %

@Temperature 257 °F
Pellets cured MDR TC95 + 15 min, 70 hr; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -23.0 °C
-9.40 °F
Temperature Retraction, TR-10