Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746A |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746A |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | |
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® H6030 High Density Polyethylene ApplicationsALATHON H 6030 is a homopolymer that provides enhanced processability, excellent stiffness and short molding cycles. Typical applications include thin wall and deep-drawRegulatory Statu.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® M4612 High Density Polyethylene ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
LyondellBasell Alathon® M4661 High Density Polyethylene ApplicationsALATHON M 4661, formerly known as LYHD 060, exhibits excellent impact, warp and environmental stress crack resistance. Typical applications are closures, institutional seating and consum.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® M5363 High Density Polyethylene ApplicationsALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properti.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Regulatory StatusThe base resin LR 7320 meets t.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | molding; ASTM D746 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
LyondellBasell Ultrathene® UE672102 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | F<sub>50</sub>; ASTM D746 |
LyondellBasell Alathon® H5234 High Density Polyethylene ApplicationsALATHON H 5234 is a high flow injection molding grade of resin designed for fast cycle and thin wall molding. It provides cold temperature impact resistance. Typical applications inclu.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | Procedure A; ASTM D746 |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | Procedure A; ASTM D746 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | Procedure A; ASTM D746 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | Procedure A; ASTM D746 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Teknor Apex TELCAR® 1050-80 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Visico™/Visico™ ME4425/LE4438 Polyethylene Visico™ ME4425 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ ME4425 and Visico™ LE4438 is a combination of a Visico™ bas.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
DuPont 20 Series 2020T Specialty Polyethylene Resin DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Visico™/Ambicat™ LE4427/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4427 / Ambicat™ LE4476 is a silane crosslinkable black compound designed for weather resistant covering/insulation of overhead and façade cables. The black base material Visico™ LE442.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Dow Engage® 8100 Polyolefin Elastomer Description: Engage® 8100 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer ap.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Dow Engage® 8130 Polyolefin Elastomer Description: Engage® 8130 polyolefin elastomer is an ethyleneoctene copolymer with low density and a high melt index. This combination provides excellent toughness, flexibility, and ease in process.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Dow Engage® 8452 Polyolefin Elastomer Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Dow AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA) AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional .. |
|||
Brittleness Temperature | -76.0 - -38.0 °C | -105 - -36.4 °F | Average value: -73.6 °C Grade Count:40 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Brittleness Temperature | <= -76.0 °C | <= -105 °F | ASTM D746 |
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables Borstar® LE8707 is a black linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufa.. |