Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 3.00 mm |
176 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.70 mm |
176 °F @Thickness 0.0669 in |
UL 746 |
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.70 mm |
176 °F @Thickness 0.0669 in |
UL 746 |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information .. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and .. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=1.50 mm |
176 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=1.70 mm |
176 °F @Thickness >=0.0669 in |
|
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=3.10 mm |
176 °F @Thickness >=0.122 in |
|
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.850 mm |
176 °F @Thickness >=0.0335 in |
|
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.850 mm |
176 °F @Thickness >=0.0335 in |
|
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1201HP-21 Polycarbonate Resin Description: LUPOY PC 1201HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=1.00 mm |
176 °F @Thickness >=0.0394 in |
|
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=1.50 mm |
176 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, High Impact, Chemical ResistanceApplication: IT/OA (M/P Battery Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information prov.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness >=3.20 mm |
176 °F @Thickness >=0.126 in |
|
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.889 mm |
176 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1015 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.889 mm |
176 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1017 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.889 mm |
176 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1002 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.889 mm |
176 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1003 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.40 mm |
176 °F @Thickness 0.0551 in |
UL 746 |
Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.889 mm |
176 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1011 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |