Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.50 mm |
140 °F @Thickness >=0.0984 in |
|
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.50 mm |
140 °F @Thickness >=0.0984 in |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.50 mm |
140 °F @Thickness >=0.0984 in |
|
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.10 mm |
140 °F @Thickness >=0.0827 in |
|
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY HG5000B PC/ABS, Heat Resistance Description: Injection Molding, PC/ABS, High Gloss, Heat Resistance, High FlowApplication: E&E (housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.60 mm |
140 °F @Thickness >=0.0630 in |
|
LG Chemical LUPOY HR5007AE PC/ABS, High Impact Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |