Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY66-GP1 General Purpose Nylon 66 General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR2 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.800 mm |
149 °F @Thickness 0.0315 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.810 mm |
149 °F @Thickness 0.0319 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=3.00 mm |
149 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST811HS NC010 Nylon 6
(Unverified Data**) Zytel® ST811HS is a flexible, heat stabilized Super Tough polyamide 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores and fastene.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG5K PA66, 25% Glass Filled, Injection Molded AG5 is a Heat and Hydrolytically Stabilized, 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
|
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
|
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.20 mm |
149 °F @Thickness 0.0472 in |
ALL |
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 3.00 mm |
149 °F @Thickness 0.118 in |
NC |
Eurostar Starflam RF0055E PA66/6, 25% Glass Filled, Injection Molded Starflam RF0055E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z250EM)Information provided by Polym.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
|
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL746B |
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.810 mm |
149 °F @Thickness 0.0319 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont .. |