Thermal Properties Metric English Comments
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746
PolyOne Maxxam™ FR PP FR 7B01 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
UL RTI, Electrical 110 °C

@Thickness 1.70 mm
230 °F

@Thickness 0.0669 in
UL 746
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Electrical 110 °C

@Thickness 1.70 mm
230 °F

@Thickness 0.0669 in
UL 746
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Electrical 110 °C

@Thickness 1.70 mm
230 °F

@Thickness 0.0669 in
UL 746
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor..
UL RTI, Electrical 110 °C

@Thickness >=0.710 mm
230 °F

@Thickness >=0.0280 in
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Electrical 110 °C

@Thickness >=1.50 mm
230 °F

@Thickness >=0.0591 in
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Electrical 110 °C

@Thickness >=0.710 mm
230 °F

@Thickness >=0.0280 in
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Electrical 110 °C

@Thickness >=1.50 mm
230 °F

@Thickness >=0.0591 in
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Electrical 110 °C

@Thickness >=1.50 mm
230 °F

@Thickness >=0.0591 in
LG Chemical LUCEL N145LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical
UL RTI, Electrical 110 °C

@Thickness >=1.00 mm
230 °F

@Thickness >=0.0394 in
LG Chemical Lupox® TE5006F PET+PC
Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical
UL RTI, Electrical 110 °C

@Thickness >=1.50 mm
230 °F

@Thickness >=0.0591 in
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL746B
Mitsubishi Xantar® MX 1000 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL746B
Mitsubishi Xantar® MX 1002 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® MX 1002 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
UL RTI, Electrical 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
UL RTI, Electrical 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform..