Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific) |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10R-(V) 10 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | GWIT |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL SE0 PPE+HIPS (Europe-Africa-Middle East) NORYL SE0 is an unfilled, flame retardant material with a Vicat B/120 of 130C according ISO 306. NORYL SE0 is V0 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Europe-Africa-Middle East) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Glow Wire Test | 775 °C @Thickness 0.800 mm |
1430 °F @Thickness 0.0315 in |
ignition temperature; ISO 60695-2-13 |
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Glow Wire Test | 775 - 960 °C | 1430 - 1760 °F | Average value: 866 °C Grade Count:3 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |