Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 103 PC (Europe-Africa-Middle East) LEXAN 103 is a high viscosity U.V. stabilized multi purpose grade. LEXAN 103 is available in transparent, translucent and opaque colours. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 121R PC (Europe-Africa-Middle East) LEXAN 121R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 121R is available in transparent, translucent and opaque colours. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East) LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri.. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm |
1560 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANTEC PC M75R Polycarbonate, Steam Resistant Information provided by Polykemi AB |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 9945A PC (Europe-Africa-Middle East) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® HP1R PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount o.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® HPX8REU PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® LS2 PC (Europe-Africa-Middle East) LEXAN LS2 is a medium viscosity grade especially designed for applications with high optical requirements in terms of clarity and light transmission. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® LUX2110T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2110T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit.. |
|||
Glow Wire Test | 850 °C @Thickness 1.50 mm |
1560 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Asia Pacific) Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® ML3021A PC (Europe-Africa-Middle East) LEXAN ML3021A is a high viscosity, UV stabilised grade especially designed for injection blow moulding and profile extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
LG Chemical Lupoy 1301-10 Polycarbonate Resin Description: LUPOY PC 1301-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Glow Wire Test | 850 °C | 1560 °F | GWFI; IEC 60695 |
Polyram RamLloy PZF301G4 PC/PBT Alloy, 20% Glass Fiber 20% Glass fiber reinforced, impact modified PC/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm |
1560 °F @Thickness 0.0787 in |
I.E.C. 695-2-1 |
Cossa Polimeri ESTACARB 1001 Polycarbonate General purpose polycarbonateHigh impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Glow Wire Test | 850 °C | 1560 °F | CEI 60695/2/1 |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Glow Wire Test | 850 °C @Thickness 1.60 mm |
1560 °F @Thickness 0.0630 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH DNH15025 GF10 Polypropylene Homopolymer, Flame Retardant, Halogen Free, Glass Fibre-Reinforced Information provided by Polykemi AB |