Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 150 °C | 302 °F | UL 746B |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
UL RTI, Electrical | 150 °C | 302 °F | UL 746B |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
UL RTI, Electrical | 150 °C | 302 °F | UL 746B |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
UL RTI, Electrical | 150 °C | 302 °F | UL 746B |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
UL RTI, Electrical | 150 °C | 302 °F | UL 746 |
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically.. |
|||
UL RTI, Electrical | 150 - 220 °C | 302 - 428 °F | Average value: 211 °C Grade Count:127 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
UL RTI, Electrical | 150 °C | 302 °F | Average value: 150 °C Grade Count:6 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |
|||
UL RTI, Electrical | 150 °C | 302 °F | Average value: 150 °C Grade Count:8 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.50 mm |
302 °F @Thickness 0.0591 in |
ALL |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
UL RTI, Electrical | 150 °C @Thickness 0.840 mm |
302 °F @Thickness 0.0331 in |
BK |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.47 mm |
302 °F @Thickness 0.0579 in |
|
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.57 mm |
302 °F @Thickness 0.0618 in |
|
Plenco 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 506 is a two-stage, mineral-filled phenolic molding compound. It is formulated for automotive ashtrays and for appliance applications such as utensil handles receiving repeated exposure to .. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.47 mm |
302 °F @Thickness 0.0579 in |
|
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.57 mm |
302 °F @Thickness 0.0618 in |
|
Plenco 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 7021 is the replacement material for the former Union Carbide BMRS-7021. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.63 mm |
302 °F @Thickness 0.0642 in |
|
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 202 is a two-stage, woodflour-filled .. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.57 mm |
302 °F @Thickness 0.0618 in |
|
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 506 is a two-stage, mineral-filled ph.. |
|||
UL RTI, Electrical | 150 °C | 302 °F | 1.60 mm |
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber.. |
|||
UL RTI, Electrical | 150 °C | 302 °F | UL 746B |
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
UL RTI, Electrical | 150 °C | 302 °F | |
Arlon 44981R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene UL Recognition File: E54153.. |
|||
UL RTI, Electrical | 150 °C | 302 °F | |
Resinoid 1312 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
UL RTI, Electrical | 150 °C | 302 °F | |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
UL RTI, Electrical | 150 °C | 302 °F | UL 746B |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.47 mm |
302 °F @Thickness 0.0579 in |
|
Plaslok 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.47 mm |
302 °F @Thickness 0.0579 in |
|
Plaslok 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
UL RTI, Electrical | 150 °C | 302 °F | 1.47 mm |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
UL RTI, Electrical | 150 °C @Thickness 1.50 mm |
302 °F @Thickness 0.0591 in |
(ALL) |
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed
&n Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-.. |
|||
UL RTI, Electrical | 150 °C | 302 °F | 1.57 mm |
Plaslok 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 204 is a two-stage, woodflour and min.. |
|||
UL RTI, Electrical | 150 °C | 302 °F | 1.57 mm |
Plaslok 7021 Black Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7021 is the replacement material for .. |