Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746C |
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation .. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5111 PEI 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific) Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Europe-Africa-Middle East) NORYL 731 is an unfilled material, with a Vicat B/120 of 140C according ISO 306. NORYL 731 is a general purpose material with good balance of Strength, Impact and Flow. NORYL 731 is available in all.. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Noryl 731H PPE+PS High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
UL RTI, Electrical | 105 °C @Thickness 0.780 mm |
221 °F @Thickness 0.0307 in |
UL 94 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
UL RTI, Electrical | 105 °C | 221 °F | 0.030 inch sample |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |
|||
UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
UL RTI, Electrical | 105 °C | 221 °F | 0.030 inch sample |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |
|||
UL RTI, Electrical | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
UL746B |
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
UL RTI, Electrical | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® 8351 HS BK 102 PA6 (Dry) Description: Ultramid 8351 HS BK-102 is a heat stabilized, pigmented black, impact modified type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughn.. |
|||
UL RTI, Electrical | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |
|||
UL RTI, Electrical | 105 °C | 221 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
UL RTI, Electrical | 105 °C | 221 °F | 0.030 inch sample |
A. Schulman POLYFLAM™ RPP 1174 Talc Filled, Homopolymer Polypropylene DescriptionPolyflam® RPP 1174 is a high performance talc filled homopolymer polypropylene product with UL V0 flammability and 105°C temperature index at 0.81 mm. RPP 1174 is non-dripping and has .. |