Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | >= 245 °C | >= 473 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Unannealed; ISO 75-2 |
PolyOne Bergamid™ PA66 C20 Black Polyamide 66 (Nylon 66) Product code EM00000364BIInformation provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Samyang Tripet® 2550GN45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced, Flame Retardant
(discontinue TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Nilit Polynil® P50L Externally Lubricated Nylon 66 Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Kolon KOPA® KN333HB30BL Hybrid Nylon 66 Hybrid, dimensionally stableApplications Timing belt coversInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75-1,-2 |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 3.20 mm |
473 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 3.20 mm |
473 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific) LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 6.40 mm |
473 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA 10% Glass Reinforced PPE+PA Alloy. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 6.40 mm |
473 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific) GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | DIN 53461 |
Polyram PlusTek PA305G6 Nylon 6.6, 30% Glass Fiber Heat stabilized, improved surface quality, 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Ter Hell Plastic Terez® PA 6.6 HT 7110 GF 41 FL-HF/2 Polyamide 66 Copolymer, 41% Glass Fiber Description: Partly aromatic Polyamide 6.6 Copolymer, 41% glass fiber reinforced and flame retardants.Application:Stiff molding parts with high stiffness by outstanding thermal stability, reduced w.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 515CS BK575M PET Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Bf |
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Bf |
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Staramide AS10 PA66, 50% Glass Bead Reinforced, Injection Molding Staramide AS10 is a 50% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO R75 |
Arkema Group Orgalloy® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | HDT/B; ISO 75-1/2 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Cheng Yu Plastic FRCV100 Flame Retardant Nylon 66, 10% Mineral Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | |
LATI Latilub 67-10STE21 G/20 PA66, 20% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66), impact modified. Silicone / PTFE. Toughened. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |