Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75 |
Nilit FRIANYL C73 H-GV15 Nylon 6.6/6 for injection molding, 15% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANMID 6 B12^ F25 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | |
Radici Radiflam® S RV250FR (cond.) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO data |
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANMID 6 B13^ F30 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C @Thickness 6.40 mm |
419 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75-1,-2 |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C @Thickness 6.40 mm |
419 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PBT-RG15 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75-1/-2 |
Lanxess Durethan® BKV 50 H2.0 901510 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C @Thickness 6.40 mm |
419 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific) 40% GR, increased strength/stiffness vs unreinforced. Non-flame retardant. For appliance handles, spotlights, electric motors, pump housings etc.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C @Thickness 3.20 mm |
419 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C @Thickness 3.20 mm |
419 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ASTM D648 |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® A5626 30% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ASTM D648 |
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | DIN 53461 |
Polyram PlusTek PB320G3 Nylon 6, 15% Glass Fiber, Flame Retardant 15% glass-fiber reinforced, flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75-1/-2 |
DSM Akulon® K224-LGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | dry; ISO 75-1/-2 |
DSM Akulon® Ultraflow K-FPG8 PA6-I-GF40 Glass Reinforced, High flow |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ASTM D648 |
Clariant Renol R60G33HSL Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75 |
Eurotec® Tecomid® MB40 GR20 NL PA6, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | HDT/B; ISO 75-2 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75 |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75 |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75-1/-2 |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ASTM D648 |
Beijing Ranger Chem PBT-201-G20 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ASTM D648 |
Beijing Ranger Chem PBT-201-G30 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |