Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | 2°C/min unannealed; ASTM D648 |
Plaskolite Optix® Acrylic Sheet Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.18 mm |
205 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
SABIC PP 524P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 524P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 6005 PC/ABS-Blend Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 and ISO 75 |
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Global CPP-110 10% CaC03 Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ISO 75-1,-2 |
Ineos ABS Lustran® ABS 450 Injection Molding Grade Lustran® ABS 450 has medium impact strength, high flow, and is injection molding grade. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Annealed, 80°C, 4 hours; ISO 75 |
LG Chemical PI-642 ABS, Fitting, High Strength Information Provided by LG Chem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Europe-Africa-Middle East) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East) Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HIPS 1000 FR-E Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
Stratasys® ABS-M30i ABS-M30i is a high strength material well suited for the medical, pharmaceutical
and food packaging industries. Parts manufactured with ABS-M30i material
are biocompatible (ISO 10993 certified) an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ISO 75-2 |
Borealis BH374MO Polypropylene Copolymer BH374MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. Products molded with this grade exhibi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 20A Nanoclay Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | |
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe) Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |