Techmer ES HiFill FR® HIPS 1000 FR-E

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® HIPS 1000 FR-E.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.045 cm/cm

@Thickness 3.17 mm
0.045 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell L 60
60
ASTM D785
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 26.2 MPa
3800 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched >= 4.27 J/cm

@Thickness 3.17 mm
>= 8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C
35.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 21.7 kV/mm
550 kV/in
Method A (Short-Time); ASTM D149