Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | 75/Method Bf |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CR120CL Polypropylene, Random Copolymer, Clarified, Lubricated Random clarified copolymer specially formulated to achieve high clarity and excellent color and color stability with excellent mold release properties. Applications: Injection molding applications s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 4.00 mm |
178 °F @Thickness 0.157 in |
after annealing 150°C 16 hr; ASTM D648 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Ineos T50-400 HDPE T50-400 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Ineos T50-500-171 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648-97 |
Ipiranga Petrochem PCC 0710 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
LyondellBasell Astryn SD068-4 Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, high modulus, mineral-filled, blow molding and extrusion grade polypropylene copolymer, good melt strength, excellent processability, excellent impact and stiffne.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Entec Hypro™ PP-CP4/2 Impact Copolymer, 4 Melt Flow This is intended for use in injection molding applications for automotive and consumer products and also contains a long term heat aging additive package.Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Entec Hypro™ PP-CP8/6 Impact Copolymer, 8 Melt Flow This product is intended for use in injection molding applications for automotive and consumer products and also contains a long-term heat aging additive package.Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Diamond Polymers NPP25-0620 Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Dow DS6D21 Polypropylene Random Copolymer Resin OverviewConsistent processabilityHigh clarity and glossComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D21 Polypropylene Resin is intended for use in case film processes. It is particularly su.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648 |
Dow DS6D21 Polypropylene Resin DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Busine.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM-D648 |
Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer PCD 0810 is a high melt flow rate heterophasic copolymer developed for injection molding applications. The product combines high impact strength and good processability with a fair stiffness level. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Injection Grade Polystyrene Compounded Resin, Injection Molding AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | |
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |