Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 - 80.0 °C | 165 - 176 °F | with 160°C Thermal Postcure; ASTM D648 |
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Petromont 1000 High Density Polyethylene Resin Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Petromont 5000 High Density Polyethylene Resin Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Solvay Engineered Polymers INDURE™ E1500 HG TPO
(discontinued **) Description: INDURE™ E1500 HG is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
LyondellBasell Alathon® H5520 High Density Polyethylene ApplicationsALATHON H 5520 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include house.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Ineos B54-25H-127 HDPE B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmenta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Ineos T50-4400 HDPE Ineos T50-4400 is a high-flow high density polyethylene copolymer intended for injection molding of thin wall containers. This material will allow for cycle time reduction while still imparting rea.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | Unannealed; ASTM D648 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C @Thickness 3.20 mm |
165 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY M3000C PP LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C @Thickness 3.20 mm |
165 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Washington Penn Medium Impact Copolymer Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C @Thickness 3.20 mm |
165 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C @Thickness 3.20 mm |
165 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Eastman DuraStar MN610 Polymer, Natural Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
ExxonMobil HDPE HD 8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 - 80.0 °C | 165 - 176 °F | with 160ºC thermal postcure; ASTM D648 |
3D Systems Accura® 50 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | |
BASF Novolen® 2700 L Polypropylene UV stabilized grade for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM-D648 |
Braskem GM8250 HDPE Blow Molding Polyethylene GM8250 is a high-density polyethylene that has high molecular weight, excellent tenacity, high stiffness, good impact resistance, and good environmental stress cracking resistance. It was developed .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM-D648 |
Braskem HD7255LS-L HDPE Injection Molding Polyethylene HD7255LS-L is a high-density polyethylene developed for injection molding. It has good tenacity and impact properties combined with good stiffness. It presents a ratio between melt flow and density .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 °C | 165 °F | ASTM D648 |
ExxonMobil Paxon™ AU55-003 Blow Molding Resin
(discontinued **) AU55-003 is a blow molding grade high density polyethylene containing an excellent antistat additive, offering a good combination of stiffness and stress crack resistance. An enhanced additive pack.. |