Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 0.125 mm |
205 °F @Thickness 0.00492 in |
unannealed; ASTM D648 |
Proto3000 ABS-M30i Fused Deposition Modeling Polymer Description: ABS-M30i is a high strength material well suited for the medical, pharmaceutical and food packaging industries. Parts manufactured with ABS-M30i material are biocompatible (ISO 10993 ce.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Europe-Africa-Middle East) PC+ABS, of non-chlorinated & non brominated flame retardant with metallic or pearlescent appearance. MAGIX color package may affect performance.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
PTS Trilac® ABS-HH2000 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
PTS Trilac® ABS-HS5500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Annealed; ISO 75-2A |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | |
Ineos ABS NOVODUR® P2L-AT ABS, Injection Grade
(discontinued **) Injection molding grade, very easy flow, antistatic, high stiffness, high gloss.Applications: Telephones, household goods, disk and video housings, office equipment.Information provided by the manuf.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
Flint Hills P4G4Z-011 Homopolymer Polypropylene Homopolymer, UL certified, USP Class VI certified, and FDA compliant.Features: Applications: Injection molding: general purpose, extruded decorative ribbon, and extruded fiber.Former Huntsman polypr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa HC-110 Modified ABS Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.35 mm |
205 °F @Thickness 0.250 in |
ASTM D648 |
IRPC Polimaxx Porene GA800 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
Stratasys® ABSplus ABSplus is up to 40 percent stronger than standard ABS material and is an ideal material for conceptual prototyping through design verification through direct digital manufacturing. The marriage of .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | HDT; ISO 75 B |
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Annealed; ASTM Data |
Dow AIM® 4800 High Impact Styrenic Resin AIM® 4800 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 25A Nanoclay Cloisite® 25A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 - 104 °C | 205 - 219 °F | |
C.O.I.M. EXTER S® S 110 Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 110: Highly reactive.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
Ashley Polymers Ashlene® PB261WO PPO A general purpose flame retardant resin for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ISO 75-2 |
CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM-D648 |
Braskem H 203 HOMO Polypropylene Homopolymer H 203 is a high melt flow rate homopolymer with a general purpose additive package. This product exhibits excellent processability and good stiffness/impact strength balance. It also features a low .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.40 mm |
205 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |