Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C @Treatment Temp. 50.0 °C, Thickness 3.18 mm |
165 °F @Treatment Temp. 122 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7005 is recommended for whites and light pastel colors only.Note: Physical properties based on L7005 tan 3210 sample.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C @Treatment Temp. 50.0 °C, Thickness 3.18 mm |
165 °F @Treatment Temp. 122 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L7007 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon L7007 is recommended for whites and light pastel colors only.Geon L7007 is a higher gloss version of L7005.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Solvay Engineered Polymers INDURE™ E1500 HG TPO
(discontinued **) Description: INDURE™ E1500 HG is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Solvay Engineered Polymers INDURE™ E1600 TPO
(discontinued **) Description: INDURE™ E1600 is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material is.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer Available in North America Recycled Content: Yes Features: CopolymerColor: Black Form: Pellets Information provided by Ravago |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
LyondellBasell Petrothene® LB560401 High Density Polyethylene ApplicationsPetrothene LB560401 exhibits good stiffness and environmental stress crack resistance. Typical applications include household chemical and personal care product bottles.Regulatory Status.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | Unannealed; ASTM D648 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Spartech 513 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Spartech 829 Static Conductive Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Spartech Spectar® Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Washington Penn Medium Impact Copolymer Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
ExxonMobil HDPE HD 8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437C30L1 Calcium Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | |
BCC Products BC 8782 Urethane Casting BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 - 171 °C | 165 - 340 °F | Average value: 154 °C Grade Count:17 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C | 165 °F | ASTM D648 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |