Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Exxon Chemical
Trade Name HDPE
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum balance of stiffness, processability and surface appearance.Availability: Latin America, North America and South America Additive: Long Term UV-15 Stabilizer: YesApplications: Consumer ArticlesRV tanksInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D4883
ESCR 100% Igepal® 10 hour
10 hour
F50; ASTM D1963A
ESCR 10% Igepal® 8.0 hour
8.0 hour
F50; ASTM D1963A
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3400 psi
(2.0 in/min); ASTM D638
Elongation at Yield 20 %
20 %
(2.0 in/min); ASTM D638
Flexural Modulus, 1% Secant 1030 MPa
150000 psi
ASTM D790B
Impact Test 78.6 J

@Thickness 3.17 mm,
Temperature -40.0 °C
58.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM
176 J

@Thickness 6.35 mm,
Temperature -56.7 °C
130 ft-lb

@Thickness 0.250 in,
Temperature -70.0 °F
ARM
Thermal Properties Metric English Comments
Melting Point <= 268 °C
<= 514 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
165 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.8 °C
109 °F
ASTM D648