Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.18 mm |
502 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 6.35 mm |
502 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Stat-Tech™ NN-20CF/000 Black HS Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 6.35 mm |
502 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | ISO 75, ASTM D648 |
Nilit Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retar.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | ISO 75, ASTM D648 |
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66 Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.20 mm |
502 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.20 mm |
502 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 LNP* LUBRICOMP* RFL36L is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXC PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXC is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RFL36SXD PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36SXD is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.20 mm |
502 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16S PA 66 LNP LUBRICOMP* RFN16S is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RFN18SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN18SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RFN1ASXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN1ASXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.20 mm |
502 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP RC008H PA 66 LNP THERMOCOMP* RC008H is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.20 mm |
502 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66 LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.20 mm |
502 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C @Thickness 3.20 mm |
502 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP VERTON RX02059 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX02059 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include; Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 70G33HS1L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L BK031 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | ASTM D648 |
A. Schulman ComAlloy Lubrilon® 636 Nylon 6/6, Carbon Fiber Reinforced, Proprietary Lubricant Package Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |