Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | >= 245 °C | >= 473 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 245 °C | >= 473 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | |
Radici Radilon® A RV150 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Samyang Tripet® 2550GN45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced, Flame Retardant
(discontinue TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 HH-FK 2020 Nylon 6.6 for injection molding, 20% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 3.20 mm |
473 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific) LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East) LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics LNP THERMOCOMP RB00A PA 66 (Europe-Africa-Middle East) 50% glass beads filled Polyamide 66 injection moulding resin. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 3.20 mm |
473 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 6.40 mm |
473 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA 10% Glass Reinforced PPE+PA Alloy. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 6.40 mm |
473 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific) GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo VYLOPET® EMC341 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo VYLOPET® EMC545 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Cheng Yu Plastic NG1150S Nylon 66, 15% Glass Fiber Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 515CS BK575M PET Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Bf |
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Bf |
Eurostar Staramide AG6ST43 PA66, 30% Glass Fiber Filled, Impact Modified, Injection Molded AG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
E-Polymers TEKAMID® JN910 PPE+PA66 10% Glass Fiber Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | |
Arkema Group Orgalloy® RS 6630 Nylon 66 Alloy, 30% Glass Fiber (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Cheng Yu Plastic FRCV100 Flame Retardant Nylon 66, 10% Mineral Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |