Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® A RV150 (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A RV150 (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
Water Absorption 7.9 %
7.9 %
Moisture Absorption at Equilibrium 2.3 %
2.3 %
Viscosity Measurement 145
145
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 5.95 GPa
863 ksi
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.650 J/cm²

@Temperature -30.0 °C
3.09 ft-lb/in²

@Temperature -22.0 °F
0.660 J/cm²

@Temperature 23.0 °C
3.14 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Vicat Softening Point 245 °C

@Load 5.10 kg
473 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 10 ohm-cm
>= 10 ohm-cm