Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANMID 6 B12^ F30 AS Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | ASTM D648 |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | ASTM D648 |
Shell Carilon® DB6G6P30 Polyketone, Lubricated, Glass-Reinforced, Injection Molding Grade
(discontinued **)&l Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYshine PBT C213 GF15 FR PBT, Glass Fiber-Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed, 0.125 in bars; ASTM D648 |
PolyOne Lubri-Tech™ NL-15CF-15GF/5M Nylon 6/12, Carbon/Glass Filled
(discontinued **) Description/Features:Carbon Fiber ReinforcedGlass Fiber ReinforcedMolybdenum Disulfide LubricatedInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C @Thickness 3.20 mm |
415 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 GF20 IM2 BK 20% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C @Thickness 3.20 mm |
415 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C @Thickness 3.20 mm |
415 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF10 L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF15 HS L BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF15 L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 GF20 L UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C @Thickness 3.20 mm |
415 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C @Thickness 3.20 mm |
415 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific) LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® A5624 20% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® N320L (Dry) Nylon 6, 20% Glass Fiber Reinforced, Lubricated, Recycled Content Features: LubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | ASTM D648 |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | ASTM D648 |
Ashley Polymers Ashlene® 527LD Nylon 66 A very high impact, slightly lubricated nylon resin.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 213 °C | 415 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP VERTON PX06418 PA 6 LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural. |