Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C @Thickness 3.18 mm |
304 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Maxxam™ PPC-10G Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C @Thickness 3.18 mm |
304 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Maxxam™ PPC-10G Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 3413R PC (Asia Pacific) Lexan* resin 3413R is a flame retardant polycarbonate grade with 30% glass fiber reinforcement to meet UL 94 V1 listing at 1.5mm. This grade can be considered for applications requiring higher stiff.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C @Thickness 6.40 mm |
304 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® 3433R PC 30% GR, provides improved mechanical properties. UV-stabilized. Internal mold release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX KS002E Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KS002E is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Electrically Conductive, Easy Molding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C @Thickness 3.20 mm |
304 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11 LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Samyang Trirex® 3025GNH15 Polycarbonate, Reinforced Flame Retardancy, Non-Halogen PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GNH15 is a reinforced, flame retardant, non-halogen grade.Applications: LCD Panel .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ISO 75 |
Teijin Panlite® GV-3430R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ISO 75-1/-2 |
Unitika A1030BRL PA6, Dry Information provided by Unitika Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 303 °F | ASTM D648 |
Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Cheng Yu Plastic ML3430 PC, 30% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ISO 75-1,-2 |
Covestro Apec® 1603 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Staramide PX08000 PA6, Impact Modified, Injection Molded Staramide PX08000 is an Impact Modified Polyamide 6 Injection Molding Resin (also known as Star X 2006)Information provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Entec Hypro™ PPC-GF40 Natural Impact Polypropylene, 40% Glass Reinforced Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0339G10M20CL Glass/Mineral Reinforced Coupled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ASTM D648 |
Ashley Polymers Ashlene® P1430 Polycarbonate, 30% Glass Reinforced A 30% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1433 with UV stabilizer.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ISO 75 -1 & -2 flat |
Asahi Kasei Tenac® 4012 Homopolymer Acetal Resin Medium viscosity grade, with reduced stiffness and increased elongation through addition of special polymersInformation provided by Asahi Kasei Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | ISO 75 |
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 151 °C | 304 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermotuf PX08000 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PX08000 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |