Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® 3413R PC (Europe-Africa-Middle East) LEXAN 3413R is a high viscosity, 30% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East) LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® XHT1141 PC (Asia Pacific) XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East) XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 - 270 °C | 292 - 518 °F | Average value: 250 °C Grade Count:34 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 6.40 mm |
291 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1200-08 Polycarbonate Resin Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1200-10 Polycarbonate Resin Description: LUPOY PC 1200-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1300-10 Polycarbonate Resin Description: LUPOY PC 1300-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 292 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PC CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | annealed; ASTM D648 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B |
Styron CALIBREâ„¢ 201-10 Polycarbonate Resin Overview: CALIBREâ„¢ 201-10 is produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. It provides excellent impact resistance, heat distortion resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B |
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B; ASTM D648 |
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Samyang Trirex® 3020U UV Stable Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020U is a high flow, UV Stable grade.Information provided by Samyang. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | 0.157 in, annealed; ASTM D648 |
Styron EMERGEâ„¢ 4310-10 Polycarbonate EMERGEâ„¢ PC 4310-10 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | 0.157 in, annealed; ASTM D648 |
Styron EMERGEâ„¢ 4330-10 Polycarbonate EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | annealed; ASTM D648 |
Styron EMERGEâ„¢ 4610-10 Polycarbonate EMERGEâ„¢ PC 4610-10 advanced resin is formulated to deliver both outstanding clarity and enhanced ignition resistance while maintaining excellent physical properties and processability. Applica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC LNP* Thermocomp* DF006 is a compound based on Polycarbonate resin containing 30% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B; ASTM D648 |
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ISO 75-1/-2 |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Ashley Polymers Ashlene® P265 PPO, 20% Glass Reinforced A general purpose, 20% glass reinforced PPO resin for injection molding applications requiring structural strength, dimensional stability and good heat resistance.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Samyang Trirex® 3020R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020R is a high flow grade with added heat stabilizers and separating materials.Informa.. |