Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 1008 T Polypropylene Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.35 mm |
216 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Trilliant™ HC HC7300-0013 ESD Black Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC (Asia Pacific) ASA+PC blend. Weatherable, injection grade. Available in a wide range of colors and is recommended for unpainted exterior applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Method A, flatwise, unannealed; ISO 75-1/2 |
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | |
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | |
Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75-1/-2 |
Lanxess Pocan® KU 2-7604 000000 PBT+PC PBT+PC, non-reinforced, injection molding, extrusion, flame retardant, impact modified, low tendency to warp |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75B |
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Spartech PE4325 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75 |
Styrolution Novodur® H605 ABS Novodur H605 is a high heat injection molding grade with enhanced flowability and reduced emission.Information provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | annealed; ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS7 BK MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75-2 |
Borealis Bormod™ BJ368MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 222 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Buckeye Polymers BP RPP 1010 TR Blk Reprocessed Polypropylene, 10% Mineral Filled Talc Filled BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin comp.. |