Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning .. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1300 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 3225 XF 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, improved flowability |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WAL34I PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WAL34I is a compound based on Polybutylene Terephalate resin containing PTFE, Aramid Fiber. Added features include Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature -20.0 - 150 °C |
72.2 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 531HS Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, Heat Shock Resistant DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SF-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 EC PA12-CD25 Product Description: Grilamid L 20 EC is an electrically conductive, medium viscosity injection molding product, based on Polyamid 12 (PA12). Grilamid L 20 EC is heat stabilized, easy to process wit.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 20 LF grey PA12 Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBAFORM C 906 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1600 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | Average above Tg, Result based on HT G22; ISO 11359 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |
|||
CTE, linear, Transverse to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 3235 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, improved flowability |