Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combinesThis data was supplied by SABIC-IP f.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC (Europe-Africa-Middle East) LNP* Lubricomp* DL002 is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC LNP LUBRICOMP* DL0029E is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 75.0 - 110 µm/m-°C | 41.7 - 61.1 µin/in-°F | Average value: 91.7 µm/m-°C Grade Count:6 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
CTE, linear, Transverse to Flow | 75.0 - 120 µm/m-°C | 41.7 - 66.7 µin/in-°F | Average value: 97.0 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
CTE, linear, Transverse to Flow | 75.0 - 97.0 µm/m-°C | 41.7 - 53.9 µin/in-°F | Average value: 89.7 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 °C |
41.7 µin/in-°F @Temperature 73.4 °F |
|
Manifattura Cattaneo RULON® 641 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
41.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY RF206AXH PA 66 LNP LUBRILOY* RF206AXH is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material include: Wear Resistant, Healthcare. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON WE003ER PBT (Europe-Africa-Middle East) LNP* Stat-kon* WE003ER is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Easy Molding, Easy Release, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX8120P PPE+PA (Europe-Africa-Middle East) GTX8120P is a glass filled extrudable Noryl GTX with low thermal conductivity, suitable for thermal breaks |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK416 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 resin for injection molding.Information provided by.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR NC010 is a 35% glass reinforced toughened heat stabilized lubricated high performance polyamide resin. It is also a P.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6H PA66, 30% Glass Filled, Injection Molded AG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined.. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 75.0 µm/m-°C | 41.7 µin/in-°F | ISO 11359 |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |