Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 150 °C |
29.4 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin Extem XH2315 Resin |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 150 °C |
29.4 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific) Extem XH2315 Resin |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 150 °C |
29.4 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East) Extem XH2315 Resin |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
CTE, linear, Transverse to Flow | 53.0 - 63.4 µm/m-°C | 29.4 - 35.2 µin/in-°F | Average value: 57.1 µm/m-°C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C | 29.4 µin/in-°F | |
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
29.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP LCL33 PEEK (Europe-Africa-Middle East) LNP* LUBRICOMP* LCL33 is a compound based on Polyethereketone resin containg Carbon Fiber, PTFE. Added features include: Elecrtically Conductive , Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
29.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear (Europe-Africa-Middle East) LNP* Lubricomp* OL004 is a compound based on PPS - Linear resin containing PTFE. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
29.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
29.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Europe-Africa-Middle East) LNP* STATKON* DEL36 is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12 LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
29.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF008AR PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF008AR is a compound based on Polyphthalamide resin, containing Glass Fiber. Added features include; Mold Release. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
29.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UX06028 PPA (Europe-Africa-Middle East) LNP * THERMOCOMP* UX06028 is a compund based on Polyphthalamide resin, containing Glass Fiber. Added features include Mold Release. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C | 29.4 µin/in-°F | TMA |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
29.4 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass/Mineral Reinforced PPA High Performance Polyamide Zytel HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is.. |
|||
CTE, linear, Transverse to Flow | 53.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
29.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON OE003A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE003A is a compound based on PPS ( branched ) resin containing Carbon Fiber. Added features include: Electrically Conductive. |