Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 52.0 - 95.0 µm/m-°C | 28.9 - 52.8 µin/in-°F | Average value: 72.3 µm/m-°C Grade Count:5 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
CTE, linear, Transverse to Flow | 52.0 - 69.0 µm/m-°C | 28.9 - 38.3 µin/in-°F | Average value: 58.0 µm/m-°C Grade Count:3 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP UX05051 PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Glass Fiber and PTFE. Added features include Heat Stabilized, Flame Retardant and Hot Water Moldable |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
28.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon OCL13 PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13 is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AX02749 ABS LNP* THERMOCOMP* AX02749 is a compound based on ABS containing proprietary fillers. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS (Europe-Africa-Middle East) LNP* Thermocomp* OF-1006 is a compound based on Polyphenylene Sulfide resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF009AS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UF009AS is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
28.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF009AXP PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF009AXP is a compound based on Polyphthalamide resin containing 45% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac RX 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594.. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | TMA |
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic Vyncolit A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bak North America, Inc. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature 20.0 °C |
28.9 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KL 1-1427 Polycarbonate/ABS Blend Glass fiber reinforced grade (30%) with high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C | 28.9 µin/in-°F | z, before Tg; IPC TM-650 2.4.24 |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
CTE, linear, Transverse to Flow | 52.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
28.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON OE002 PPS - LINEAR LNP* STAT-KON* OE002 is a compound based on PPS - Linear resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |