Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 0.000 - 100 °C |
22.2 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E381 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East) CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 40.0 - 102 µm/m-°C | 22.2 - 56.7 µin/in-°F | Average value: 61.4 µm/m-°C Grade Count:16 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 87.0 µm/m-°C | 22.2 - 48.3 µin/in-°F | Average value: 51.8 µm/m-°C Grade Count:4 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 79.0 µm/m-°C | 22.2 - 43.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 20.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | TMA |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baygal® 90 IK 51 Polyurethane Uses: Suitable for the solid insulation of measuring transducers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its ne.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® AV2 370 XT PET-GF35 35% Glass Reinforced, Applications with extremely narrow tolerances |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | z direction |
Arlon AD450A Glass, PTFE and Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | z direction |
Arlon AD410 Glass, PTFE and Micro-Dispersed Ceramic High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear, Transverse to Flow | 40.0 - 90.0 µm/m-°C | 22.2 - 50.0 µin/in-°F | Average value: 73.6 µm/m-°C Grade Count:39 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | TMA |
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)... |
|||
CTE, linear, Transverse to Flow | 40.0 - 79.0 µm/m-°C | 22.2 - 43.9 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 80.0 µm/m-°C | 22.2 - 44.4 µin/in-°F | Average value: 59.3 µm/m-°C Grade Count:21 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East) CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 50.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |