Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 39.0 - 92.0 µm/m-°C | 21.7 - 51.1 µin/in-°F | Average value: 75.0 µm/m-°C Grade Count:10 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C | 21.7 µin/in-°F | |
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C | 21.7 µin/in-°F | |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C | 21.7 µin/in-°F | ASTM D696 |
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled 35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista.. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C | 21.7 µin/in-°F | ASTM D696 |
Kuraray Genestarâ„¢ GC1201A-M41 Nylon, Glass Filled and Carbon Filled Reinforced injection grade for conductive applications.Main Features:ConductivityHeat resistanceChemical resistanceExample of applications:Quick connector |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C | 21.7 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-freeApplication Examples: mixer insert for blenders, washing machi.. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
21.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East) LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
21.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON OE008 PPS (Europe-Africa-Middle East) LNP * Stat-kon* OE 008 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include: Electically Conductive. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
21.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
21.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp EF008EXP PEI (Europe-Africa-Middle East) LNP* Thermocomp* EF008EXP is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.This data was supplied by SABIC-IP .. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature 20.0 °C |
21.7 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac RX 853G is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature 20.0 °C |
21.7 µin/in-°F @Temperature 68.0 °F |
TMA |
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac RX 865M is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
CTE, linear, Transverse to Flow | 39.0 µm/m-°C @Temperature 20.0 °C |
21.7 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America RX® 865M Novolac Phenolic Fiberglass reinforced phenolic novolac compound featuring dimensional stability, moderate impact resistance, good strength and modulus.Information provided by Vyncolit, a Sumitomo Bak Group |