Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 92.0 - 110 µm/m-°C @Temperature 100 - 200 °C |
51.1 - 61.1 µin/in-°F @Temperature 212 - 392 °F |
Average value: 101 µm/m-°C Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 °C |
51.1 µin/in-°F @Temperature 73.4 °F |
|
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 20.0 °C |
51.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical LG-703A ABS, Low Gloss, General Purpose Information Provided by LG Chem |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
51.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RL4040HSUV PA 66 LNP* LUBRICOMP* RL4040HSUV is a compound based on Nylon 66 containing 20% PTFE. Added features of this grade include: Heat Stabilized, UV Stabilized, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
51.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
51.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C | 51.1 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-40 FC PA6-GF40 Product description: Grilon BG-40 FC is a heat stabilized PA6 injection molding grade with 40% glass fibers. Grilon BG-40 FC has the following important properties: High stiffnessExcellent surface f.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C | 51.1 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler with high stiffness low warpage and low creep for sup.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
51.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
51.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
51.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
51.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
51.1 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 100KM NC000 Acetal (POM)
(Unverified Data**) Kevlar® Modified High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100KM is a high viscosity acetal homopolymer resin modified with Kevlar aramid resin. It is designed for appl.. |
|||
CTE, linear, Transverse to Flow | 92.0 µm/m-°C | 51.1 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET) Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |