Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® RCY6113 PC+ABS (Asia Pacific) Cycoloy* RCY6113 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 5VB rating @ 2.0mm an.. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DBL34E PC (Europe-Africa-Middle East) LNP* LUBRICOMP DBL34E is a compound based on Polycarbonate resin containing Glass Bead, PTFE. Added features include: Easy Molding, Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features include; Internally Lubricated, Easy Molding. |
|||
CTE, linear, Transverse to Flow | 76.0 - 100 µm/m-°C @Temperature 55.0 - 260 °C |
42.2 - 55.6 µin/in-°F @Temperature 131 - 500 °F |
Average value: 83.8 µm/m-°C Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
CTE, linear, Transverse to Flow | 76.0 - 100 µm/m-°C @Thickness 2.00 - 4.00 mm |
42.2 - 55.6 µin/in-°F @Thickness 0.0787 - 0.157 in |
Average value: 83.8 µm/m-°C Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP REL22 PA 66 LNP* LUBRICOMP* REL22 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66 LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A.. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific) This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa.. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C | 42.2 µin/in-°F | z, below Tg; IPC TM-650 2.4.24 |
Arlon 37N Polyimide Low-Flow 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir.. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature 20.0 °C |
42.2 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 60M10E5 Nylon 6 Alloy, 10% Mineral Filled (Conditioned) RS 60 series rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents). Stability of mechanical, electrical and dimensional properties.Mineral filled.. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
42.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL44 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL44 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON MV006BS PP LNP* VERTON* MV006BS is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this grade include: Heat Stabilized, Burst Pressure, Structural, Chemically Coupl.. |
|||
CTE, linear, Transverse to Flow | 76.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DL0039EF PC LNP* Lubricomp* DL-0039EF is a compound based on Polycarbonate resin containing 15% PTFE. Characteristics of this grade include: Flame Retardant and Internally Lubricated. |