Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 66.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
36.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EX1632T PC Lexan* EX1632T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and UV stabilizer. It is available .. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C @Temperature 0.000 - 200 °C |
36.7 µin/in-°F @Temperature 32.0 - 392 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater.. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon ZEL34XXC PPE+PS (Europe-Africa-Middle East) LNP* Stat-kon* ZEL34XXC is a compound based on PPE+PS Blend resin containing Carbon Fiber, PTFE. Added features include : Electrically Conductive , Internally Lubricated.This data was supplied by S.. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
36.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon DE0049 PC (Europe-Africa-Middle East) LNP* Stat-kon* DC-1004 FR is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.This.. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C | 36.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-KG6 PA410-GF30 % Glass Reinforced, Heat Stabilized, for E&E applications |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C | 36.7 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C | 36.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-HG6 PA410-GF30 30% Glass Reinforced, Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 66.0 µm/m-°C | 36.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR 30% Glass Reinforced, Flame Retardant (Halogen free) |