Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E831 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C | 30.0 µin/in-°F | |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
30.0 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL RN1300 PPE (Asia Pacific) 15% glass/mineral reinforced PPE. Nonchlorinated, nonbrominated, flame-retardant. Black and gray. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1510 compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000P PEI Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000P PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
30.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
30.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LX04015 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LX04015 is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include: Electrically Conductive |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
30.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
30.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® 940 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene Terephthalate Rynite 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength stiffness and low warpage.Informatio.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C | 30.0 µin/in-°F | z, below Tg; IPC TM-650 2.4.24 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 50.0 - 150 °C |
30.0 µin/in-°F @Temperature 122 - 302 °F |
z direction; IPC TM-650 2.4.24 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.0 µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
DuPont Performance Polymers VESPEL TP-8929 Polyimide DuPont Vespel TP-8929 parts are specified for mechanical and thermal performance. TP-8929 parts offer low friction, dimensional stability, low outgassing, radiation resistance, and creep resistance... |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
30.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV00ASXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
30.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON RV00AXX9 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AXX9 is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 Listing. Effective June, 2007 this grade will no longer.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 20.0 °C |
30.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
(discontinued **) XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
30.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF OF008I PPS - Linear (Europe-Africa-Middle East) LNP* Thermotuf* OF008I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |
|||
CTE, linear, Transverse to Flow | 54.0 µm/m-°C @Temperature -20.0 - 150 °C |
30.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer b.. |