Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 200 µm/m-°C @Temperature -40.0 - 40.0 °C |
111 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY CR3020 ASA Low-gloss ASA for profile and capstock applications |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C @Temperature -30.0 - 30.0 °C |
111 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C @Temperature -30.0 - 30.0 °C |
111 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E831 |
PolyOne Edgetek® X TR2-20GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C @Temperature 23.0 - 55.0 °C |
111 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**) Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,.. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C @Temperature 23.0 - 55.0 °C |
111 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C @Temperature -40.0 - 40.0 °C |
111 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® 1103 PBT+PC AUTOMOTIVE. Unreinforced, impact modified PBT+PC alloy. Excellent low temperature impact and chemical resistance. Range gray, black colors. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C | 111 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi.. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C | 111 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C | 111 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C | 111 µin/in-°F | ISO 11359-1,-2 |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66
(discontinued **) PA 6/66 |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C | 111 µin/in-°F | z, above Tg; IPC TM-650 2.4.24 |
Arlon 45N Multifunctional Epoxy Laminate and Prepreg Arlon 45N is a tough, high Tg (175°C by DSC) multifunctional epoxy laminate and prepreg system designed for use in a variety of higher layer count MLBs. Processable using conventional FR-4 conditi.. |
|||
CTE, linear, Transverse to Flow | 200 µm/m-°C | 111 µin/in-°F | z, above Tg; IPC TM-650 2.4.24 |
Arlon 44N Multifunctional Microdispersed Ceramic Filled Epoxy-Fiberglass Prepreg Arlon 44N is a high resin content multifunctional (175°C) epoxy prepreg system with a proprietary microdispersed ceramic filler system. 44N is engineered for the filling of clearance holes in thi.. |